OverviewThis dissertation, An Investigation of the Deformation of Anodic Aluminium Oxide Nano-honeycomb During Nanoindentation by King-yeung, Ng, 吳競洋, was obtained from The University of Hong Kong (Pokfulam, Hong Kong) and is being sold pursuant to Creative Commons: Attribution 3.0 Hong Kong License. The content of this dissertation has not been altered in any way. We have altered the formatting in order to facilitate the ease of printing and reading of the dissertation. All rights not granted by the above license are retained by the author. DOI: 10.5353/th_b4284124 Subjects: Aluminum - Anodic oxidationAluminum oxideNanostructured materials - Mechanical propertiesMetallic films - Mechanical properties Full Product DetailsAuthor: King-Yeung Ng , 吳競洋Publisher: Open Dissertation Press Imprint: Open Dissertation Press Dimensions: Width: 21.60cm , Height: 1.10cm , Length: 27.90cm Weight: 0.685kg ISBN: 9781360963044ISBN 10: 1360963049 Publication Date: 24 January 2017 Audience: General/trade , General Format: Hardback Publisher's Status: Active Availability: Temporarily unavailable The supplier advises that this item is temporarily unavailable. It will be ordered for you and placed on backorder. Once it does come back in stock, we will ship it out to you. Table of ContentsReviewsAuthor InformationTab Content 6Author Website:Countries AvailableAll regions |